General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 11.7 g/cm³ Show Material materials with Density of 11.7 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Flexural strength | 20.0 °C | 517 - 586 MPa Show Material materials with Flexural strength of 517 - 586 MPa |
Hardness, Rockwell B | 20.0 °C | 69 - 83 [-] Show Material materials with Hardness, Rockwell B of 69 - 83 [-] |
Tensile strength | 20.0 °C | 344 - 413 MPa Show Material materials with Tensile strength of 344 - 413 MPa |
Electrical
Property | Value |
---|---|
Specific Electrical conductivity | 38 - 64 % IACS Show Material materials with Specific Electrical conductivity of 38 - 64 % IACS |
Chemical properties
Property | Value |
---|---|
Copper | 48 - 52 % Show Material materials with Copper of 48 - 52 % |