DIN 3.2384 T6

Want to keep this datasheet? Save it now in your required format

Primary standard name

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

2.00E+7 - 2.30E+7 S/m

Show Material materials with Electrical conductivity of 2.00E+7 - 2.30E+7 S/m

General

PropertyTemperatureValue

Density

20.0 °C

2.68 g/cm³

Show Material materials with Density of 2.68 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

71.5 GPa

Show Material materials with Elastic modulus of 71.5 GPa

Elongation

20.0 °C

2 - 5 %

Show Material materials with Elongation of 2 - 5 %

Fracture toughness

20.0 °C

22 MPa·√m

Show Material materials with Fracture toughness of 22 MPa·√m

Tensile strength

20.0 °C

280 - 345 MPa

Show Material materials with Tensile strength of 280 - 345 MPa

Yield strength Rp0.2

20.0 °C

220 - 275 MPa

Show Material materials with Yield strength Rp0.2 of 220 - 275 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

100.0 °C

2.16E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.16E-5 1/K

Melting point

610 °C

Show Material materials with Melting point of 610 °C

Specific heat capacity

100.0 °C

963 J/(kg·K)

Show Material materials with Specific heat capacity of 963 J/(kg·K)

Thermal conductivity

20.0 °C

150 W/(m·K)

Show Material materials with Thermal conductivity of 150 W/(m·K)

Chemical properties

PropertyValue

Beryllium

0.07 %

Show Material materials with Beryllium of 0.07 %

Copper

0.2 %

Show Material materials with Copper of 0.2 %

Iron

0.2 %

Show Material materials with Iron of 0.2 %

Magnesium

0.45 - 0.7 %

Show Material materials with Magnesium of 0.45 - 0.7 %

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

Silicon

6.5 - 7.5 %

Show Material materials with Silicon of 6.5 - 7.5 %

Titanium

0.1 - 0.2 %

Show Material materials with Titanium of 0.1 - 0.2 %

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %