Unclassified Low Alloy Steel
EN 10225 Grade S420G1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10225 Grade S355G7 thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10225 Grade S420G1 thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10225 Grade S460G1 thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Other Copper Zinc Alloy
EN 1652 Grade CuZn20Al2As R390Kohlenstoffarmer Stahl
EN 10225 Grade S355G13 normalized or normalized formed (+N)Other Copper Zinc Alloy
EN 12452 Grade CuZn20Al2As O60Other Copper Zinc Alloy
EN 1652 Grade CuZn20Al2As R330Leaded Brass
EN 12164 Grade CuZn36Pb2As R280Leaded Brass
EN 12168 Grade CuZn36Pb2As H070Tin Brass
EN 12451 Grade CuZn28Sn1As O60Kohlenstoffarmer Stahl
EN 10225 Grade S355G13 quenched and tempered (+QT)Medium Carbon Steel
EN 10225 Grade S355G14 normalized or normalized formed (+N)Medium Carbon Steel
EN 10225 Grade S355G15 normalized or normalized formed (+N)Tin Brass
EN 12451 Grade CuZn28Sn1As O50Tin Brass
EN 12451 Grade CuZn28Sn1As R320Tin Brass
EN 12451 Grade CuZn28Sn1As R360Wrought Copper Brass Yellow Brass
EN 12451 Grade CuZn30As O60Wrought Copper Pure / Low Alloyed Copper
CEN/TS 13388 Grade CW009A MLeaded Brass
CEN/TS 13388 Grade CW602N R280