Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Wrought Copper High Copper Alloy
ASTM B251 Grade C17000 TD04Wrought Copper High Copper Alloy
ASTM B196 Grade C17000 TF00Wrought Copper High Copper Alloy
ASTM B196 Grade C17000 TB00Wrought Copper High Copper Alloy
ASTM B196 Grade C17000 TH04Wrought Copper High Copper Alloy
ASTM B643 Grade C17200 TH04Wrought Copper High Copper Alloy
ASTM B197 Grade C17300 TH04Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TM00Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TM02Wrought Copper High Copper Alloy
ASTM B197 Grade C17300 TD04Wrought Copper High Copper Alloy
ASTM B197 Grade C17300 TF00Wrought Copper High Copper Alloy
ASTM B197 Grade C17200 TM04Wrought Copper High Copper Alloy
ASTM B197 Grade C17200 TM06Wrought Copper High Copper Alloy
ASTM B197 Grade C17200 TM08Wrought Copper High Copper Alloy
ASTM B570 Grade C17000 TD02Wrought Copper High Copper Alloy
ASTM B570 Grade C17000 TD01Wrought Copper Nickel Silver Grade
EN 12164 Grade CuNi12Zn30Pb1 R420Nickel Chromium Molybdenum Alloy
DIN 17744 Grade NiMo16Cr16Ti solution heat-treated and quenched