Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Austenitischer rostfreier Stahl
Esshete 1250Geliefert von:
Alleima (formerly Sandvik Materials Technology)Nickel Chromium Iron Alloy
Sanicro 31HTGeliefert von:
Alleima (formerly Sandvik Materials Technology)Nickel Chromium Iron Alloy
Sanicro 30 AnnealedGeliefert von:
Alleima (formerly Sandvik Materials Technology)Nickel Chromium Iron Alloy
Sanicro 30 Cold WorkedGeliefert von:
Alleima (formerly Sandvik Materials Technology)Martensitischer Edelstahl
DIN 17440 Grade X12Cr13 soft annealed (+A)Martensitischer Edelstahl
EN 10088-1 Grade X6Cr13 soft annealed (+A)Austenitischer rostfreier Stahl
EN 10028-7 Grade X8CrNiNb16-13 solution annealed (+AT)Ferritischer Edelstahl
EN 10088-1 Grade X2CrTi17 soft annealed (+A)Martensitischer Edelstahl
DIN 17440 Grade X6Cr13 soft annealed (+A)Ferritischer Edelstahl
DIN 17456 Grade X2CrTi12 soft annealed (+A)Ferritischer Edelstahl
EN 10028-7 Grade X2CrTi17 soft annealed (+A)Ferritischer Edelstahl
EN 10312 Grade X2CrTi12 soft annealed (+A)Ferritischer Edelstahl
EN 10088-4 Grade X2CrTi12 soft annealed (+A)Austenitischer rostfreier Stahl
EN 10216-5 Grade X8CrNiNb16-13 solution annealed (+AT)Martensitischer Edelstahl
DIN 17440 Grade X10Cr13 quenched and tempered (+QT)