Kohlenstoffarmer Stahl
EN 10028-2 Grade P235GH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10025-2 Grade S235J2 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10207 Grade P275SL normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10025-3 Grade S275N normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10025-3 Grade S275NL normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10025-2 Grade S235J0 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10209 Grade DC01EK cold rolled, skin passedGeliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 12CrMoV12-10 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMoSi5-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMoV9-10 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10149-2 Grade S315MC thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10149-2 Grade S355MC thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10149-3 Grade S315NC normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10149-3 Grade S355NC normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10207 Grade P235S normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant