EN 10209 Grade DC01EK cold rolled, skin passed

Want to keep this datasheet? Save it now in your required format

Description

Cold rolled low carbon steel for flat products for vitreous enamelling (one or two coats of conventional enamelling). Application: domestic appliances (cooking, laundry), sanitary ware (bathtubs, shower trays, sinks), architectural panels (interior and exterior), signage

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³

Typical for Low Carbon Steel

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa

Typical for Low Carbon Steel

Poisson's ratio

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Low Carbon Steel

Shear modulus

82 GPa

Show Material materials with Shear modulus of 82 GPa

Typical for Low Carbon Steel

Tensile strength

20 °C

270 - 390 MPa

Show Material materials with Tensile strength of 270 - 390 MPa

cold rolled, skin passed

EN 10209

Sheet

Transverse

20 °C

270 - 390 MPa

Show Material materials with Tensile strength of 270 - 390 MPa

cold rolled, skin passed

EN 10209

Strip, Bar

Yield strength

20 °C

140 - 310 MPa

Show Material materials with Yield strength of 140 - 310 MPa

cold rolled, skin passed

EN 10209

Sheet

Transverse

20 °C

140 - 290 MPa

Show Material materials with Yield strength of 140 - 290 MPa

cold rolled, skin passed

EN 10209

Sheet

Transverse

20 °C

140 - 270 MPa

Show Material materials with Yield strength of 140 - 270 MPa

cold rolled, skin passed

EN 10209

Sheet

Transverse

20 °C

140 - 270 MPa

Show Material materials with Yield strength of 140 - 270 MPa

cold rolled, skin passed

EN 10209

Strip, Bar

Unlock all property charts

Thermal

PropertyValueComment

Coefficient of thermal expansion

1.32e-05 - 1.38e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.32e-05 - 1.38e-05 1/K

Typical for Low Carbon Steel

Max service temperature

500 °C

Show Material materials with Max service temperature of 500 °C

Typical for Carbon Steel

Melting point

1480 - 1526 °C

Show Material materials with Melting point of 1480 - 1526 °C

Typical for Low Carbon Steel

Specific heat capacity

465 J/(kg·K)

Show Material materials with Specific heat capacity of 465 J/(kg·K)

Typical for Low Carbon Steel

Thermal conductivity

25 - 93 W/(m·K)

Show Material materials with Thermal conductivity of 25 - 93 W/(m·K)

Typical for Low Carbon Steel

Electrical

PropertyValueComment

Electrical resistivity

1.43e-07 - 1.74e-07 Ω·m

Show Material materials with Electrical resistivity of 1.43e-07 - 1.74e-07 Ω·m

Typical for Carbon Steel

Magnetic

PropertyValueComment

Curie temperature

770 °C

Show Material materials with Curie temperature of 770 °C

Typical for Low Carbon Steel

Chemical properties

PropertyValueConditionRelated StandardsShape

Carbon

0.08

Show Material materials with Carbon of 0.08

cold rolled, skin passed

EN 10209

Sheet

Manganese

0.6

Show Material materials with Manganese of 0.6

cold rolled, skin passed

EN 10209

Sheet

Phosphorus

0.045

Show Material materials with Phosphorus of 0.045

cold rolled, skin passed

EN 10209

Sheet

Sulfur

0.05

Show Material materials with Sulfur of 0.05

cold rolled, skin passed

EN 10209

Sheet