General
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Density | 1.08 g/cm³ Show Supplier Material materials with Density of 1.08 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 1.4 % Show Supplier Material materials with Moisture absorption of 1.4 % | 50%RH | ISO 62 | 2 mm | |
Water absorption | 3.2 % Show Supplier Material materials with Water absorption of 3.2 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 1.3 GPa Show Supplier Material materials with Elastic modulus of 1.3 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
2.4 GPa Show Supplier Material materials with Elastic modulus of 2.4 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Elongation | 40 % Show Supplier Material materials with Elongation of 40 % | dry | ISO 527-2/1A | 50mm/min | nominal | |
100 % Show Supplier Material materials with Elongation of 100 % | 50%RH | ISO 527-2/1A | min. | 50mm/min | nominal | ||
Elongation at yield | 4.6 % Show Supplier Material materials with Elongation at yield of 4.6 % | dry | ISO 527-2/1A | 50mm/min | |
15 % Show Supplier Material materials with Elongation at yield of 15 % | 50%RH | ISO 527-2/1A | 50mm/min | ||
Flexural modulus | 2.2 GPa Show Supplier Material materials with Flexural modulus of 2.2 GPa | dry | ISO 178 | 2mm/min | |
Flexural strength | 85 MPa Show Supplier Material materials with Flexural strength of 85 MPa | dry | ISO 178 | 2mm/min | |
Impact strength, Charpy notched | -30 °C | 4.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4.5 kJ/m² | dry | ISO 179/1eA | |
-30 °C | 7.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 7.5 kJ/m² | 50%RH | ISO 179/1eA | ||
23 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 9 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 9 kJ/m² | 50%RH | ISO 179/1eA | ||
Impact strength, Charpy unnotched | No Break at 23°C | dry | ISO 179/1eU | ||
Yield strength | 45 MPa Show Supplier Material materials with Yield strength of 45 MPa | 50%RH | ISO 527-2/1A | 50mm/min | |
65 MPa Show Supplier Material materials with Yield strength of 65 MPa | dry | ISO 527-2/1A | 50mm/min |
Thermal
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 0.00011 1/K Show Supplier Material materials with Coefficient of thermal expansion of 0.00011 1/K | ISO 11359-1/-2 | 23°C-55°C | ||
0.00011 1/K Show Supplier Material materials with Coefficient of thermal expansion of 0.00011 1/K | ISO 11359-1/-2 | 23°C-55°C, Transverse | |||
Heat deflection temperature | 65 °C Show Supplier Material materials with Heat deflection temperature of 65 °C | ISO 75/2Af | 1.80 MPa | ||
160 °C Show Supplier Material materials with Heat deflection temperature of 160 °C | ISO 75/2Bf | 0.45 MPa | |||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | ISO 11357-1/-3 | 10°C/min | ||
Vicat softening temperature | 185 °C Show Supplier Material materials with Vicat softening temperature of 185 °C | ISO 306 | 50°C/h 50N | ||
Flammability | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Shrinkage | 1 % Show Supplier Material materials with Shrinkage of 1 % | 270/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
1.2 % Show Supplier Material materials with Shrinkage of 1.2 % | 270/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Deep black | |
Features | Heat Stabilized | |
Processing methods | Injection Molding |