XENOY™ Resin 5720U

Want to keep this datasheet? Save it now in your required format

Description

Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.17 g/cm³

Show Material materials with Density of 1.17 g/cm³

ASTM D 792

Water absorption

23.0 °C

0.08 %

Show Material materials with Water absorption of 0.08 %

ISO 62 | 23°C, 50% RH

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.83 GPa

Show Material materials with Elastic modulus of 1.83 GPa

ASTM D 638 | 5 mm/min

Elongation

23.0 °C

122.4 %

Show Material materials with Elongation of 122.4 %

ASTM D 638 | Type I, 5 mm/min

Elongation at yield

23.0 °C

4.6 %

Show Material materials with Elongation at yield of 4.6 %

ASTM D 638 | Type I, 5 mm/min

Flexural modulus

23.0 °C

1.86 GPa

Show Material materials with Flexural modulus of 1.86 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

69 MPa

Show Material materials with Flexural strength of 69 MPa

ASTM D 790 | 1.3 mm/min, 50 mm span

Flexural yield strength

23.0 °C

71 MPa

Show Material materials with Flexural yield strength of 71 MPa

ISO 178 | 2 mm/min

Impact strength, Charpy notched

-30.0 °C

47 kJ/m²

Show Material materials with Impact strength, Charpy notched of 47 kJ/m²

ISO 179/1eA

23.0 °C

55 kJ/m²

Show Material materials with Impact strength, Charpy notched of 55 kJ/m²

ISO 179/1eA

Impact strength, Izod notched

-40.0 °C

46 kJ/m²

Show Material materials with Impact strength, Izod notched of 46 kJ/m²

ISO 180/1A

-30.0 °C

48 kJ/m²

Show Material materials with Impact strength, Izod notched of 48 kJ/m²

ISO 180/1A

-20.0 °C

50 kJ/m²

Show Material materials with Impact strength, Izod notched of 50 kJ/m²

ISO 180/1A

-10.0 °C

52 kJ/m²

Show Material materials with Impact strength, Izod notched of 52 kJ/m²

ISO 180/1A

23.0 °C

55 kJ/m²

Show Material materials with Impact strength, Izod notched of 55 kJ/m²

ISO 180/1A

Unlock all property charts

Impact strength, Izod notched, ASTM

-40.0 °C

598 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 598 J/m

ASTM D 256

-30.0 °C

647 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 647 J/m

ASTM D 256

-20.0 °C

695 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 695 J/m

ASTM D 256

-10.0 °C

663 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 663 J/m

ASTM D 256

23.0 °C

722 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 722 J/m

ASTM D 256

Unlock all property charts

Tensile strength

23.0 °C

50 MPa

Show Material materials with Tensile strength of 50 MPa

ASTM D 638 | Type I, 5 mm/min

Yield strength

23.0 °C

44 MPa

Show Material materials with Yield strength of 44 MPa

ASTM D 638 | Type I, 5 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

9.75E-5 1/K

Show Material materials with Coefficient of thermal expansion of 9.75E-5 1/K

ASTM E 831 | -40°C to 95°C

Coefficient of thermal expansion, transverse

23.0 °C

1E-4 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 1E-4 1/K

ASTM E 831 | -40°C to 95°C

Heat deflection temperature, 0.45 MPa

109 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 109 °C

ISO 75/Bf | 0.45 MPa

Vicat softening temperature

119 °C

Show Material materials with Vicat softening temperature of 119 °C

ASTM D 1525 | Rate B/50

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

11 g/10min

Show Material materials with Melt mass-flow rate of 11 g/10min

ISO 1133 | 250°C/5 kg

Melt volume-flow rate

18 cm³/10min

Show Material materials with Melt volume-flow rate of 18 cm³/10min

ISO 1133 | 265°C/5.0 kg

Shrinkage

23.0 °C

1 - 1.2 %

Show Material materials with Shrinkage of 1 - 1.2 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

ATM/Ticket Machine,Auto Aftermarket,City,Data Transfer,Document Handling,Electronic Components,Enclosure/Housing/Cover,Enclosures,Exterior Rail Components,Heavy Vehicles,Individual Equiptment,Industrial Material Handling,Lab Ware and Clinical Diagnostics,Lawn/Garden,Medical Device,Motorcycle,Rear/Signal Lighting,Security/Detection,Wireless Communications,Wire & cable

Processing methods

Drying Temperature: 110°C, Drying Time: 4-6hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 260-275°C, Nozzle Temperature: 255-270°C, Front - Zone 3 Temperature: 255-275°C, Middle - Zone 2 Temperature: 250-270°C, Rear - Zone 1 Temperature: 245-265°C, Mold Temperature: 65-90°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 50-80rpm, Shot to Cylinder Size: 50-80%, Vent Depth: 0.013-0.02mm