RADILON A HS 164 NT

Alternative and trade names
PA66
Want to keep this datasheet? Save it now in your required format

Description

PA66 injection moulding grade, internally lubricated and fast cycling. General purpose grade, suitable for parts requiring high productivity like fasteners, connectors, cable ties.

This material data has been provided by Radici Group.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.14 g/cm³

Show Supplier Material materials with Density of 1.14 g/cm³

ISO 1183

Moisture absorption

23.0 °C

2.1 %

Show Supplier Material materials with Moisture absorption of 2.1 %

ISO 62, 50% RH, thickness tested (mm): 2

Water absorption

23.0 °C

8.9 %

Show Supplier Material materials with Water absorption of 8.9 %

ISO 62, 2mm

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

3 GPa

Show Supplier Material materials with Elastic modulus of 3 GPa

ISO 527-2/1A, 1mm/min

Elongation

23.0 °C

30 %

Show Supplier Material materials with Elongation of 30 %

ISO 527-2/1A, 50mm/min

Elongation at yield

23.0 °C

4.6 %

Show Supplier Material materials with Elongation at yield of 4.6 %

ISO 527-2/1A

Flexural modulus

23.0 °C

2.8 GPa

Show Supplier Material materials with Flexural modulus of 2.8 GPa

ISO 178, 2mm/min

Flexural strength

23.0 °C

110 MPa

Show Supplier Material materials with Flexural strength of 110 MPa

ISO 178, 2mm/min

Impact strength, Charpy notched

-30.0 °C

4.5 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 4.5 kJ/m²

ISO 179/1eU

23.0 °C

5 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m²

ISO 179/1eU

Yield strength

23.0 °C

80 MPa

Show Supplier Material materials with Yield strength of 80 MPa

ISO 527-2/1A, 50mm/min

Impact strength, Charpy unnotched

No Break, ISO 179/1eU

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

9.5E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 9.5E-5 1/K

ISO 11359-1/-2, 23°C-55°C

Coefficient of thermal expansion, transverse

23.0 °C

9.4E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 9.4E-5 1/K

ISO 11359-1/-2, 23°C-55°C

Heat deflection temperature, 0.45 MPa

200 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 200 °C

ISO 75/2Bf

Heat deflection temperature, 1.80 MPa

70 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 70 °C

ISO 75/2Af

Melting point

260 °C

Show Supplier Material materials with Melting point of 260 °C

ISO 11357-1/3

Vicat softening temperature

240 °C

Show Supplier Material materials with Vicat softening temperature of 240 °C

ISO 306, 50°C/h 50N

Flammability

for 0.8mm, V2 UL94 and for for 0.4mm, V2 UL94

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

IEC 60112, Sol.A

Surface resistivity

23.0 °C

1.00E+12 Ω/sq

Show Supplier Material materials with Surface resistivity of 1.00E+12 Ω/sq

IEC 60093, 500V

Volume resistivity

23.0 °C

1.00E+15 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm

IEC 60093, 500V

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

1.2 %

Show Supplier Material materials with Shrinkage of 1.2 %

ISO 294-4

Shrinkage, transverse

23.0 °C

1.3 %

Show Supplier Material materials with Shrinkage, transverse of 1.3 %

ISO 294-4

Technological properties

Property
Certifications

RoHS 2011/65/UE

Color

Natural

Processing methods

Injection Molding