General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 70 % Show Supplier Material materials with Bio-based content of 70 % | dry | ASTM D6866-12 Method B |
Density | 1.09 g/cm³ Show Supplier Material materials with Density of 1.09 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.9 % Show Supplier Material materials with Moisture absorption of 1.9 % | dry | Sim. to ISO 62 |
Water absorption | 5.8 % Show Supplier Material materials with Water absorption of 5.8 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 1.6 GPa Show Supplier Material materials with Elastic modulus of 1.6 GPa | conditioned | ISO 527-1/-2 | |
3.2 GPa Show Supplier Material materials with Elastic modulus of 3.2 GPa | dry | ISO 527-1/-2 | ||
120 °C | 0.6 GPa Show Supplier Material materials with Elastic modulus of 0.6 GPa | dry | ISO 527-1/-2 | |
140 °C | 0.52 GPa Show Supplier Material materials with Elastic modulus of 0.52 GPa | dry | ISO 527-1/-2 | |
Elongation | 20 % Show Supplier Material materials with Elongation of 20 % | dry | ISO 527-1/-2 | |
50 % Show Supplier Material materials with Elongation of 50 % | conditioned | ISO 527-1/-2 | ||
120 °C | 200 % Show Supplier Material materials with Elongation of 200 % | dry | ISO 527-1/-2 | |
140 °C | 200 % Show Supplier Material materials with Elongation of 200 % | dry | ISO 527-1/-2 | |
Elongation at yield | 4.6 % Show Supplier Material materials with Elongation at yield of 4.6 % | dry | ISO 527-1/-2 | |
20 % Show Supplier Material materials with Elongation at yield of 20 % | conditioned | ISO 527-1/-2 | ||
Impact strength, Charpy notched | -30 °C | 4 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m² | dry | ISO 179/1eA |
-30 °C | 4.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4.5 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 5.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 5.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m² | conditioned | ISO 179/1eA | |
Tensile strength | 45 MPa Show Supplier Material materials with Tensile strength of 45 MPa | conditioned | ISO 527-1/-2 | |
55.0 MPa Show Supplier Material materials with Tensile strength of 55.0 MPa | dry | ISO 527-1/-2 | ||
120 °C | 38 MPa Show Supplier Material materials with Tensile strength of 38 MPa | dry | ISO 527-1/-2 | |
140 °C | 32 MPa Show Supplier Material materials with Tensile strength of 32 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Heat deflection temperature | 75 °C Show Supplier Material materials with Heat deflection temperature of 75 °C | dry | ISO 75-1/-2 | 2 MPa | |
175 °C Show Supplier Material materials with Heat deflection temperature of 175 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 250 °C Show Supplier Material materials with Melting point of 250 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt mass-flow rate | 280 °C | 24 g/10min Show Supplier Material materials with Melt mass-flow rate of 24 g/10min | dry | ISO 1133 |
Melt volume-flow rate | 280 °C | 26 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 26 cm³/10min | dry | ISO 1133 |
Viscosity number | 170 cm³/gr Show Supplier Material materials with Viscosity number of 170 cm³/gr | dry | ISO 307, 1157, 1628 |