Kohlenstoffarmer Stahl
EN 10028-2 Grade P295GH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Chromium Molybdenum Steel
EN 10028-2 Grade 12CrMo9-10 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-3 Grade P460NL1 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10083-3 Grade 20MnB5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant