Molybdenum Steel
EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Chromium Molybdenum Steel
EN 10028-2 Grade 10CrMo9-10 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Wrought Copper High Copper Alloy
ASTM B251 Grade C17000 TD04Wrought Copper High Copper Alloy
ASTM B196 Grade C17000 TF00