Biegemodul: 5.7 - 6.7 GPa

Quick Comparison

Polyamide 46 (PA46)

Stanyl® TE250F6

Geliefert von:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TS250F6D

Geliefert von:

DSM Engineering Materials

Polycarbonat (PC)

LNP™ THERMOCOMP™ Compound D251

Geliefert von:

Sabic

Polyamide 46 (PA46)

Stanyl® TW250F6

Geliefert von:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW200F8

Geliefert von:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW241F10

Geliefert von:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K222-KMV5

Geliefert von:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW241F8

Geliefert von:

DSM Engineering Materials

Polycarbonat (PC)

LNP™ THERMOCOMP™ Compound D251RC

Geliefert von:

Sabic

Polymermischung (Blend)

VALOX™ FR Resin ENH8530 - Europe

Geliefert von:

Sabic

Polybutylenterephthalat (PBT)

VALOX™ FR Resins DR48

Polyamide 6 (PA6)

Akulon® K224-HG7

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

Minlon® 22C NC010

Polybutylenterephthalat (PBT)

Crastin® SK603 NC010

Polyamide 46 (PA46)

Stanyl® TE200F8

Geliefert von:

DSM Engineering Materials

Polyvinylidenefluoride (PVDF)

Kynar® 370

Geliefert von:

Arkema: High Performance Polymers

Polyamide 6 (PA6)

Akulon® K223-HM6

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

Akulon® S223-HG6

Geliefert von:

DSM Engineering Materials

Polymermischung (Blend)

Crastin® LW9020 NC010