Härte, Brinell: 17 [-]

Quick Comparison

Wrought Copper Brass Yellow Brass

EnviB 1 - CuZn40 - CW509L / C28000

Geliefert von:

Lebronze Alloys

Chromium Molybdenum Steel

JIS G3221 Grade SFCM780R

Nickel Chromium Molybdenum Steel

ASTM A487 Grade 2 Class C, Heat-Treated