General
Property | Value |
---|---|
Carbon Footprint | Scope 1&2 (direct and indirect smelter emissions) - less than 4 T CO₂ eq/ T Al, average 2,6 T CO₂ eq / T Al. Total carbon footprint from cradle to gate is less than 8 T CO₂ eq / T Al. |
Dimension
Property | Value |
---|---|
Dimensions | Weight: 10 kg, 16 kg |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elongation A50 | 0 - 8 % Show Supplier Material materials with Elongation A50 of 0 - 8 % at 23.0 °C | 23.0 °C | according to DIN EN 1706 |
Hardness, Brinell | 0 - 90 [-] Show Supplier Material materials with Hardness, Brinell of 0 - 90 [-] at 23.0 °C | 23.0 °C | according to DIN EN 1706 |
Tensile strength | 0 - 320 MPa Show Supplier Material materials with Tensile strength of 0 - 320 MPa at 23.0 °C | 23.0 °C | according to DIN EN 1706 |
Yield strength Rp0.2 | 0 - 220 MPa Show Supplier Material materials with Yield strength Rp0.2 of 0 - 220 MPa at 23.0 °C | 23.0 °C | according to DIN EN 1706 |
Chemical properties
Property | ||
---|---|---|
Aluminium | Balance | |
Copper | 0.2 - 0.7 % | |
Iron | 0 - 0.25 % | |
Magnesium | 0.25 - 0.45 % | |
Other | 0 - 0.1 % | |
Silicon | 6.5 - 7.5 % | |
Titanium | 0 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Engine Head | |
Processing history | Smelters: Khakas Aluminium Smelter (KhAZ), Irkutsk Aluminium Smelter (IrKAZ) |