General
Property | Value |
---|---|
Carbon Footprint | Scope 1&2 (direct and indirect smelter emissions) - less than 4 T CO₂ eq / T Al, average 2,6 T CO₂ eq / T Al. Total carbon footprint from cradle to gate is less than 8 T CO₂ eq / T Al. |
Dimension
Property | Value |
---|---|
Dimensions | Weight: 7 kg, 10 kg, 15 kg, 16 kg |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elongation A50 | 0 - 8 % Show Supplier Material materials with Elongation A50 of 0 - 8 % at 23.0 °C | 23.0 °C | according to DIN EN 1706 |
Hardness, Brinell | 0 - 90 [-] Show Supplier Material materials with Hardness, Brinell of 0 - 90 [-] at 23.0 °C | 23.0 °C | according to DIN EN 1706 |
Tensile strength | 0 - 320 MPa Show Supplier Material materials with Tensile strength of 0 - 320 MPa at 23.0 °C | 23.0 °C | according to DIN EN 1706 |
Yield strength | 160 - 230 MPa Show Supplier Material materials with Yield strength of 160 - 230 MPa at 23.0 °C | 23.0 °C | |
Yield strength Rp0.2 | 0 - 220 MPa Show Supplier Material materials with Yield strength Rp0.2 of 0 - 220 MPa at 23.0 °C | 23.0 °C | according to DIN EN 1706 |
Chemical properties
Property | ||
---|---|---|
Aluminium | Balance | |
Iron | 0 - 0.55 % | |
Magnesium | 0.2 - 0.65 % | |
Other | 0 - 0.15 % | |
Silicon | 6.5 - 7.5 % | |
Titanium | 0 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Wheels | |
Processing history | Smelters: Sayanogorsk Aluminium Smelter (SAZ), Khakas Aluminium Smelter (KHAZ), Irkutsk Aluminium Smelter (IrKAZ), Krasnoyarsk Aluminium Smelter (KRAZ) |