Härte, Brinell: 183 - 241 [-]

Quick Comparison

Kohlenstoffarmer Stahl

EN 10028-3 Grade P275NH normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Kohlenstoffarmer Stahl

EN 10028-3 Grade P355NH normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Kohlenstoffarmer Stahl

EN 10207 Grade P275SL normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Chromium Molybdenum Steel

EN 10028-2 Grade 10CrMo9-10 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMo4-5 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 12CrMo9-10 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Molybdenum Steel

EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Kohlenstoffarmer Stahl

EN 10149-3 Grade S260NC normalized or normalized formed (+N)

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10149-2 Grade S315MC thermomechanically rolled

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10149-2 Grade S355MC thermomechanically rolled

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10149-3 Grade S315NC normalized or normalized formed (+N)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10025-5 Grade S355J2W normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Unclassified Low Alloy Steel

EN 10025-5 Grade S355K2W normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Kohlenstoffarmer Stahl

EN 10326 Grade S250GD cold rolled

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10326 Grade S280GD cold rolled

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10326 Grade S320GD cold rolled

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10326 Grade S350GD cold rolled

Geliefert von:

1 Matmatch-Lieferant

Unclassified Carbon Steel

ASTM A516 Grade 380 As-Rolled or Normalized and/or Stress Relieved

Geliefert von:

1 Matmatch-Lieferant

Unclassified Stainless Steel

ASTM A537 Class 1 Normalized

Geliefert von:

2 Matmatch-Lieferanten

Seite 1 von 81