Impact strength, Izod notched, ASTM: 750 J/m

Quick Comparison

Polycarbonat (PC)

LNP™ THERMOCOMP™ Compound DX14354X

Geliefert von:

Sabic

Polycarbonat (PC)

LEXAN™ Resin PK2870

Polycarbonat (PC)

LNP™ THERMOTUF™ Compound D1000UF

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ COLORCOMP™ Compound DX04401H

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ THERMOCOMP™ Compound DX11354

Geliefert von:

Sabic

Polybuten (PB)

Poly(butene-1) PB

Polycarbonat (PC)

LEXAN™ Copolymer FXEMPX1 - Asia

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ ELCRIN™ EXL8483RCC

Geliefert von:

Sabic

Polybutylenterephthalat (PBT)

XENOY™ Resin HX6600HP

Polybutylenterephthalat (PBT)

XENOY™ Resin HX5600HP

Polycarbonat (PC)

LEXAN™ Resin EM1210