Schubmodule: 73 - 78 GPa

Quick Comparison

Chromium Molybdenum Steel

EN 10028-2 Grade 10CrMo9-10 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMo4-5 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Molybdenum Steel

EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Medium Carbon Steel

EN 10028-3 Grade P355N normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

EN 10028-4 Grade X12Ni5 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 10CrMo9-10 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMo4-5 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Nickel molybdenum Steel

EN 10028-2 Grade 15NiCuMoNb5-6-4 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

EN 10028-4 Grade 11MnNi5-3 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

EN 10028-4 Grade 13MnNi6-3 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

EN 10028-4 Grade 15NiMn6 normalized or normalized formed (+N)

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

EN 10083-3 Grade 30MnB5 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Martensitischer Edelstahl

ASTM A841 Grade A Class 1 Thermo-Mechanical Control Process (TMCP)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

ASTM A353 Double-Normalized and Tempered

Geliefert von:

1 Matmatch-Lieferant

Austenitischer rostfreier Stahl

ASTM A276 Grade S20910 Annealed
Seite 1 von 172