Streckgrenze Rp 0,2: 287 MPa

Quick Comparison

Kohlenstoffarmer Stahl

EN 10028-2 Grade P355GH normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Kohlenstoffarmer Stahl

EN 10028-3 Grade P355NH normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

5000 Serie

EN 573-3 Grade AW-5154A H18

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 10CrMo9-10 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMo4-5 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 12CrMo9-10 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10028-3 Grade P460NH normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

3000 Serie

EN 573-3 Grade AW-3004 H19

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10028-6 Grade P355QH quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10028-6 Grade P460QH quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

2000 Serie

EN 573-3 Grade AW-2024 T3

Geliefert von:

1 Matmatch-Lieferant

2000 Serie

EN 573-3 Grade AW-2024 T3

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

7000 Serie

WL 3.4364-1 Grade 3.4365 T6

Geliefert von:

3 Matmatch-Lieferanten

7000 Serie

WL 3.4364-1 Grade 3.4365 T6

Geliefert von:

3 Matmatch-Lieferanten

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00

2000 Serie

EN 573-3 Grade AW-2024 T351

Geliefert von:

1 Matmatch-Lieferant

2000 Serie

EN 573-3 Grade AW-2024 T351

Geliefert von:

1 Matmatch-Lieferant

Seite 1 von 16