Kohlenstoffarmer Stahl
EN 10028-2 Grade P355GH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10028-3 Grade P355NH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Nickel Molybdenum Steel
EN 10028-2 Grade 20MnMoNi4-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMoSi5-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-3 Grade P460NH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Unclassified Low Alloy Steel
EN 10028-6 Grade P355QH quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-6 Grade P460QH quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-6 Grade P500QH quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF002000 Serie
EN 573-3 Grade AW-2014 T62000 Serie
EN 573-3 Grade AW-2014 T6