Chromium Molybdenum Steel
EN 10028-2 Grade 12CrMo9-10 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
2000 Serie
EN 573-3 Grade AW-2014 T62000 Serie
EN 573-3 Grade AW-2014 T62000 Serie
EN 573-3 Grade AW-2014 T6512000 Serie
EN 573-3 Grade AW-2014 T651Austenitischer rostfreier Stahl
EN 10088-1 Grade X2CrNiMoN17-13-3 solution annealed (+AT)Austenitischer rostfreier Stahl
DIN 17440 Grade X2CrNiMoN17-13-3 solution heat-treated and quenchedAustenitischer rostfreier Stahl
EN 10088-1 Grade X2CrNiMoN17-11-2 solution annealed (+AT)Austenitischer rostfreier Stahl
DIN 17440 Grade X2CrNiMoN17-13-3 quenched (+Q)Austenitischer rostfreier Stahl
EN 10028-7 Grade X2CrNiMoN17-13-3 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10088-1 Grade X1CrNiMoCuN25-25-5 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X2CrNiMoN17-11-2 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X3CrNiMoBN17-13-3 solution annealed (+AT)Ferritischer Edelstahl
EN 10028-7 Grade X2CrNi12 soft annealed (+A)Austenitischer rostfreier Stahl
EN 10216-5 Grade X2CrNiMoN17-13-3 solution annealed (+AT)Ferritischer Edelstahl
EN 10028-7 Grade X6CrNiTi12 soft annealed (+A)