Streckgrenze Rp 0,2: 490 - 710 MPa

Quick Comparison

Kohlenstoffarmer Stahl

EN 10152 Grade DC06 skin passed

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10025-2 Grade E295 normalized or normalized formed (+N)

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10025-2 Grade E360 normalized or normalized formed (+N)

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10152 Grade DC01 skin passed

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10152 Grade DC03 skin passed

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10152 Grade DC05 skin passed

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10209 Grade DC01EK cold rolled, skin passed

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10209 Grade DC04EK cold rolled, skin passed

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10209 Grade DC06EK cold rolled, skin passed

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

ISO 683-1 Grade C45E quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10083-3 Grade 20MnB5 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Kohlenstoffarmer Stahl

ASTM A517 Grade F Quenched and Tempered

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10025-6 Grade S550QL1 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10025-6 Grade S620QL1 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10025-6 Grade S690QL1 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10111 Grade DD12 hot rolled

Geliefert von:

1 Matmatch-Lieferant

Seite 1 von 55