Kohlenstoffarmer Stahl
EN 10028-2 Grade P235GH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10028-2 Grade P265GH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10028-2 Grade P295GH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10025-2 Grade S355J0C as-rolled condition (+AR)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 normalized and tempered (+NT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMoSi5-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10120 Grade P245NB normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10120 Grade P265NB normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Molybdenum Steel
EN 10028-2 Grade 18MnMo4-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Nickel Steel
EN 10028-4 Grade 12Ni14 normalized and tempered (+NT)Geliefert von:
1 Matmatch-Lieferant
Nickel Steel
EN 10028-4 Grade 15NiMn6 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
ASTM A841 Grade B Class 1 Thermo-Mechanical Control Process (TMCP)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
ASTM A612 As-Rolled or Normalized and/or Stress RelievedGeliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10216-2 Grade 12CrMo9-10 quenched and tempered (+QT)Unclassified Low Alloy Steel
ISO 683-2 Grade 33MnCrB5-2 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
ASTM A542 Type A Class 2 Quenched and TemperedGeliefert von:
1 Matmatch-Lieferant