General
Property | Value | Comment |
---|---|---|
Density | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastic modulus | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Low Carbon Steel | |||
Elongation | 17.2 % Show Material materials with Elongation of 17.2 % | Predicted Value, A80 | |||
18 % Show Material materials with Elongation of 18 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate | A200 | |
19.2 % Show Material materials with Elongation of 19.2 % | Predicted Value, Transverse | ||||
20.0 % Show Material materials with Elongation of 20.0 % | Predicted Value, A80 Transverse | ||||
22 % Show Material materials with Elongation of 22 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate | A50 | |
24.9 % Show Material materials with Elongation of 24.9 % | Predicted Value | ||||
Hardness, Brinell | 243 [-] Show Material materials with Hardness, Brinell of 243 [-] | Predicted Value, Transverse | |||
Poisson's ratio | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Low Carbon Steel | |||
Reduction of area | 40.1 % Show Material materials with Reduction of area of 40.1 % | Predicted Value | |||
44.1 % Show Material materials with Reduction of area of 44.1 % | Predicted Value, Transverse | ||||
Shear modulus | 82 GPa Show Material materials with Shear modulus of 82 GPa | Typical for Low Carbon Steel | |||
Shear strength | 553.7 MPa Show Material materials with Shear strength of 553.7 MPa | Predicted Value | |||
Tensile strength | 450 - 585 MPa Show Material materials with Tensile strength of 450 - 585 MPa | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate | |
485 - 620 MPa Show Material materials with Tensile strength of 485 - 620 MPa | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate | ||
Yield strength | 263.7 MPa Show Material materials with Yield strength of 263.7 MPa | Predicted Value, RP1 | |||
310 MPa Show Material materials with Yield strength of 310 MPa | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate | ||
317.9 MPa Show Material materials with Yield strength of 317.9 MPa | Predicted Value, RP1 Transverse | ||||
345 MPa Show Material materials with Yield strength of 345 MPa | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate | ||
366.4 MPa Show Material materials with Yield strength of 366.4 MPa | Predicted Value, Transverse | ||||
368.8 MPa Show Material materials with Yield strength of 368.8 MPa | Predicted Value, RP02 | ||||
373.8 MPa Show Material materials with Yield strength of 373.8 MPa | Predicted Value, RP05 | ||||
407.4 MPa Show Material materials with Yield strength of 407.4 MPa | Predicted Value, RP002 | ||||
462.1 MPa Show Material materials with Yield strength of 462.1 MPa | Predicted Value, RP02 Transverse |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.32e-05 - 1.38e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Max service temperature | 303.3 °C Show Material materials with Max service temperature of 303.3 °C | Predicted Value, Long |
500 °C Show Material materials with Max service temperature of 500 °C | Typical for Carbon Steel | |
Melting point | 1480 - 1526 °C Show Material materials with Melting point of 1480 - 1526 °C | Typical for Low Carbon Steel |
Specific heat capacity | 465 J/(kg·K) Show Material materials with Specific heat capacity of 465 J/(kg·K) | Typical for Low Carbon Steel |
Thermal conductivity | 25 - 93 W/(m·K) Show Material materials with Thermal conductivity of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Electrical
Property | Value | Comment |
---|---|---|
Electrical conductivity | 6 S/m Show Material materials with Electrical conductivity of 6 S/m | Predicted Value |
Electrical resistivity | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with Electrical resistivity of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnetic
Property | Value | Comment |
---|---|---|
Curie temperature | 770 °C Show Material materials with Curie temperature of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Carbon | 0.15 % Show Material materials with Carbon of 0.15 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Chromium | 0.25 % Show Material materials with Chromium of 0.25 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Copper | 0.35 % Show Material materials with Copper of 0.35 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Manganese | 0.7 - 1.35 % Show Material materials with Manganese of 0.7 - 1.35 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Molybdenum | 0.3 % Show Material materials with Molybdenum of 0.3 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Nickel | 0.6 % Show Material materials with Nickel of 0.6 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Niobium | 0.03 % Show Material materials with Niobium of 0.03 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Silicon | 0.15 - 0.5 % Show Material materials with Silicon of 0.15 - 0.5 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Vanadium | 0.06 % Show Material materials with Vanadium of 0.06 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |