Reines Titan
DIN 17850 Grade Ti1Pd AnnealedAustenitischer rostfreier Stahl
EN 10088-1 Grade X2CrNiMoN17-13-3 solution annealed (+AT)Austenitischer rostfreier Stahl
DIN 17440 Grade X2CrNiMoN17-13-3 solution heat-treated and quenchedAustenitischer rostfreier Stahl
EN 10088-1 Grade X3CrNiMo17-13-3 solution annealed (+AT)Austenitischer rostfreier Stahl
DIN 17440 Grade X6CrNiTi18-10 solution heat-treated and quenchedAustenitischer rostfreier Stahl
EN 10088-1 Grade X2CrNiMoN17-11-2 solution annealed (+AT)Austenitischer rostfreier Stahl
DIN 17440 Grade X6CrNiMoTi17-12-2 solution heat-treated and quenchedAustenitischer rostfreier Stahl
DIN 17440 Grade X2CrNiMoN17-13-3 quenched (+Q)Austenitischer rostfreier Stahl
DIN 17440 Grade X6CrNiTi18-10 quenched (+Q)Austenitischer rostfreier Stahl
EN 10272 Grade X1NiCrMoCu31-27-4 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10272 Grade X2CrNiMoN17-11-2 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10272 Grade X2CrNiMoN17-13-3 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10088-1 Grade X2CrNiMo17-12-3 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10272 Grade X2CrNi18-9 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X2CrNiMoN17-13-3 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X6CrNiTi18-10 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X6CrNiMoTi17-12-2 solution annealed (+AT)