Streckgrenze: 625 - 655 MPa

Quick Comparison

Kohlenstoffarmer Stahl

EN 10152 Grade DC01 skin passed

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10152 Grade DC03 skin passed

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10152 Grade DC04 skin passed

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10152 Grade DC05 skin passed

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10209 Grade DC01EK cold rolled, skin passed

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10209 Grade DC04EK cold rolled, skin passed

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10209 Grade DC06EK cold rolled, skin passed

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10083-3 Grade 20MnB5 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10025-6 Grade S620QL1 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10025-6 Grade S690QL1 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10025-6 Grade S620Q quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10025-6 Grade S620QL quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10025-6 Grade S690Q quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10025-6 Grade S690QL quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10028-6 Grade P690QL1 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10028-6 Grade P690QL2 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10028-6 Grade P690Q quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10028-6 Grade P690QH quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

Wrought Copper Nickel Silver Grade

UNS C77000 boway

Geliefert von:

Ningbo Boway Alloy Material
Seite 1 von 12