Austenitischer rostfreier Stahl
DIN 17480 Grade X60CrMnMoVNbN21-10 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
EN 10090 Grade X33CrNiMnN23-8 solution heat-treated and precipitation hardened (+AT+P)Martensitischer Edelstahl
EN 10090 Grade X40CrSiMo10-2 quenched and tempered (+QT)Martensitischer Edelstahl
EN 10090 Grade X45CrSi9-3 quenched and tempered (+QT)Austenitischer rostfreier Stahl
EN 10090 Grade X50CrMnNiNbN21-9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
EN 10090 Grade X53CrMnNiN21-9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
EN 10090 Grade X53CrMnNiNbN21-9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
EN 10090 Grade X55CrMnNiN20-8 solution heat-treated and precipitation hardened (+AT+P)Martensitischer Edelstahl
EN 10090 Grade X85CrMoV18-2 quenched and tempered (+QT)Austenitischer rostfreier Stahl
DIN 17480 Grade X 45 CrNiW 18 9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
DIN 17480 Grade X50CrMnNiNbN21-9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
DIN 17480 Grade X53CrMnNiN21-9 solution heat-treated and precipitation hardened (+AT+P)Martensitischer Edelstahl
DIN 17480 Grade X45CrSi9-3 quenched and tempered (+QT)Martensitischer Edelstahl
DIN 17480 Grade X85CrMoV18-2 quenched and tempered (+QT)