DIN 17480 Grade X 45 CrNiW 18 9 solution heat-treated and precipitation hardened (+AT+P)

Want to keep this datasheet? Save it now in your required format

Description

X45CrNiW18-9 is an austenitic Cr-Ni-W-alloyed valve steel. The steel shows sufficient corrosion resistance in exhaust condensate and good resistance to lead compounds at increased temperatures. Application at operating temperatures up to 730 deg. Use: exhaust valves, valves

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.9 g/cm³

Show Material materials with Density of 7.9 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

205 GPa

Show Material materials with Elastic modulus of 205 GPa

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Austenitic Stainless Steel

Shear modulus

23.0 °C

77 GPa

Show Material materials with Shear modulus of 77 GPa

Typical for Austenitic Stainless Steel

Tensile strength

500.0 °C

600 MPa

Show Material materials with Tensile strength of 600 MPa

550.0 °C

550 MPa

Show Material materials with Tensile strength of 550 MPa

600.0 °C

500 MPa

Show Material materials with Tensile strength of 500 MPa

650.0 °C

410 MPa

Show Material materials with Tensile strength of 410 MPa

700.0 °C

350 MPa

Show Material materials with Tensile strength of 350 MPa

750.0 °C

270 MPa

Show Material materials with Tensile strength of 270 MPa

800.0 °C

180 MPa

Show Material materials with Tensile strength of 180 MPa

Yield strength Rp0.2

500.0 °C

250 MPa

Show Material materials with Yield strength Rp0.2 of 250 MPa

550.0 °C

230 MPa

Show Material materials with Yield strength Rp0.2 of 230 MPa

600.0 °C

210 MPa

Show Material materials with Yield strength Rp0.2 of 210 MPa

650.0 °C

190 MPa

Show Material materials with Yield strength Rp0.2 of 190 MPa

700.0 °C

170 MPa

Show Material materials with Yield strength Rp0.2 of 170 MPa

750.0 °C

140 MPa

Show Material materials with Yield strength Rp0.2 of 140 MPa

800.0 °C

100 MPa

Show Material materials with Yield strength Rp0.2 of 100 MPa

Unlock all property charts

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

1.55E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.55E-5 1/K

300.0 °C

1.75E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.75E-5 1/K

500.0 °C

1.82E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.82E-5 1/K

700.0 °C

1.86E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.86E-5 1/K

Unlock all property charts

Max service temperature, long

0 - 730 °C

Show Material materials with Max service temperature, long of 0 - 730 °C

Melting point

1230 - 1480 °C

Show Material materials with Melting point of 1230 - 1480 °C

Typical for Austenitic Stainless Steel

Specific heat capacity

20.0 °C

500 J/(kg·K)

Show Material materials with Specific heat capacity of 500 J/(kg·K)

Thermal conductivity

20.0 °C

14.5 W/(m·K)

Show Material materials with Thermal conductivity of 14.5 W/(m·K)

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

8.5E-7 Ω·m

Show Material materials with Electrical resistivity of 8.5E-7 Ω·m

Typical for Austenitic Stainless Steel

Chemical properties

PropertyValue

Carbon

0.4 - 0.5 %

Show Material materials with Carbon of 0.4 - 0.5 %

Chromium

17 - 19 %

Show Material materials with Chromium of 17 - 19 %

Manganese

0.8 - 1.5 %

Show Material materials with Manganese of 0.8 - 1.5 %

Nickel

8 - 10 %

Show Material materials with Nickel of 8 - 10 %

Phosphorus

0.05 %

Show Material materials with Phosphorus of 0.05 %

Silicon

2 - 3 %

Show Material materials with Silicon of 2 - 3 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Tungsten

0.8 - 1.2 %

Show Material materials with Tungsten of 0.8 - 1.2 %