General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 8.1 g/cm³ Show Material materials with Density of 8.1 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 20.0 °C | 215 GPa Show Material materials with Elastic modulus of 215 GPa |
Elongation | 20.0 °C | 15 % Show Material materials with Elongation of 15 % |
Hardness, Rockwell C | 20.0 °C | 32 [-] Show Material materials with Hardness, Rockwell C of 32 [-] |
Reduction of area | 20.0 °C | 25 % Show Material materials with Reduction of area of 25 % |
Tensile strength | 20.0 °C | 1100 - 1400 MPa Show Material materials with Tensile strength of 1100 - 1400 MPa |
500.0 °C | 1050 MPa Show Material materials with Tensile strength of 1050 MPa | |
550.0 °C | 1030 MPa Show Material materials with Tensile strength of 1030 MPa | |
600.0 °C | 1000 MPa Show Material materials with Tensile strength of 1000 MPa | |
650.0 °C | 930 MPa Show Material materials with Tensile strength of 930 MPa | |
700.0 °C | 820 MPa Show Material materials with Tensile strength of 820 MPa | |
750.0 °C | 680 MPa Show Material materials with Tensile strength of 680 MPa | |
800.0 °C | 500 MPa Show Material materials with Tensile strength of 500 MPa | |
Yield strength Rp0.2 | 20.0 °C | 725 MPa Show Material materials with Yield strength Rp0.2 of 725 MPa |
500.0 °C | 700 MPa Show Material materials with Yield strength Rp0.2 of 700 MPa | |
550.0 °C | 650 MPa Show Material materials with Yield strength Rp0.2 of 650 MPa | |
600.0 °C | 650 MPa Show Material materials with Yield strength Rp0.2 of 650 MPa | |
650.0 °C | 600 MPa Show Material materials with Yield strength Rp0.2 of 600 MPa | |
700.0 °C | 600 MPa Show Material materials with Yield strength Rp0.2 of 600 MPa | |
750.0 °C | 500 MPa Show Material materials with Yield strength Rp0.2 of 500 MPa | |
800.0 °C | 450 MPa Show Material materials with Yield strength Rp0.2 of 450 MPa | |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.19E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.19E-5 1/K |
300.0 °C | 1.31E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.31E-5 1/K | |
500.0 °C | 1.37E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.37E-5 1/K | |
700.0 °C | 1.45E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.45E-5 1/K | |
Specific heat capacity | 20.0 °C | 460 J/(kg·K) Show Material materials with Specific heat capacity of 460 J/(kg·K) |
Thermal conductivity | 20.0 °C | 13 W/(m·K) Show Material materials with Thermal conductivity of 13 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 1 - 1.8 % Show Material materials with Aluminium of 1 - 1.8 % |
Boron | 8E-3 % Show Material materials with Boron of 8E-3 % |
Carbon | 0.04 - 0.1 % Show Material materials with Carbon of 0.04 - 0.1 % |
Chromium | 18 - 21 % Show Material materials with Chromium of 18 - 21 % |
Cobalt | 2 % Show Material materials with Cobalt of 2 % |
Copper | 0.2 % Show Material materials with Copper of 0.2 % |
Iron | 3 % Show Material materials with Iron of 3 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Nickel | 65 % Show Material materials with Nickel of 65 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |
Titanium | 1.8 - 2.7 % Show Material materials with Titanium of 1.8 - 2.7 % |