Austenitischer rostfreier Stahl
DIN 17445 Grade G-X5CrNiMoNb18-10 quenched (+Q)Austenitischer rostfreier Stahl
DIN 17445 Grade G-X5CrNiNb18-9 quenched (+Q)Austenitischer rostfreier Stahl
DIN 17445 Grade G-X6CrNi18-9 quenched (+Q)Austenitischer rostfreier Stahl
DIN 17445 Grade G-X6CrNiMo18-10 quenched (+Q)Martensitischer Edelstahl
DIN 17445 Grade G-X20Cr14 quenched and tempered (+QT)Austenitischer rostfreier Stahl
DIN 17445 Grade G-X3CrNiMoN17-13-5 quenched (+Q)Martensitischer Edelstahl
DIN 17445 Grade G-X5CrNi13-4 quenched and tempered (+QT1)Martensitischer Edelstahl
DIN 17445 Grade G-X8CrNi13 quenched and tempered (+QT)Austenitischer rostfreier Stahl
EN 10213-4 Grade GX5CrNi19-10 solution heat-treated and quenchedAustenitischer rostfreier Stahl
EN 10213-4 Grade GX5CrNiMo19-11-2 solution heat-treated and quenchedFerritischer Edelstahl
DIN 17445 Grade G-X22CrNi17 quenched and tempered (+QT)Austenitischer rostfreier Stahl
EN 10213-4 Grade GX5CrNiNb19-11 solution heat-treated and quenchedAustenitischer rostfreier Stahl
EN 10213-4 Grade GX2CrNiMo19-11-2 solution heat-treated and quenchedAustenitischer rostfreier Stahl
EN 10213-4 Grade GX2NiCrMo28-20-2 solution heat-treated and quenchedAustenitischer rostfreier Stahl
EN 10213-4 Grade GX5CrNiMoNb19-11-2 solution heat-treated and quenchedAustenitischer rostfreier Stahl
EN 10213-4 Grade GX2CrNi19-11 solution heat-treated and quenchedDuplex rostfreier Stahl
EN 10213-4 Grade GX2CrNiMoCuN25-6-3-3 solution heat-treated and quenchedDuplex rostfreier Stahl
EN 10213-4 Grade GX2CrNiMoN22-5-3 solution heat-treated and quenchedDuplex rostfreier Stahl
EN 10213-4 Grade GX2CrNiMoN26-7-4 solution heat-treated and quenched