General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.7 g/cm³ Show Material materials with Density of 7.7 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 220 GPa Show Material materials with Elastic modulus of 220 GPa | Typical for Ferritic Stainless Steel |
Elongation | 20.0 °C | 4 % Show Material materials with Elongation of 4 % | |
Hardness, Brinell | 20.0 °C | 230 - 300 [-] Show Material materials with Hardness, Brinell of 230 - 300 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Ferritic Stainless Steel |
Shear modulus | 23.0 °C | 77 GPa Show Material materials with Shear modulus of 77 GPa | Typical for Ferritic Stainless Steel |
Tensile strength | 20.0 °C | 780 - 980 MPa Show Material materials with Tensile strength of 780 - 980 MPa | |
Yield strength Rp0.2 | 20.0 °C | 590 MPa Show Material materials with Yield strength Rp0.2 of 590 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1E-5 1/K Show Material materials with Coefficient of thermal expansion of 1E-5 1/K | |
200.0 °C | 1.05E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.05E-5 1/K | ||
300.0 °C | 1.1E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.1E-5 1/K | ||
400.0 °C | 1.1E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.1E-5 1/K | ||
500.0 °C | 1.1E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.1E-5 1/K | ||
Melting point | 1425 - 1530 °C Show Material materials with Melting point of 1425 - 1530 °C | Typical for Ferritic Stainless Steel | |
Specific heat capacity | 20.0 °C | 460 J/(kg·K) Show Material materials with Specific heat capacity of 460 J/(kg·K) | |
Thermal conductivity | 20.0 °C | 25 W/(m·K) Show Material materials with Thermal conductivity of 25 W/(m·K) |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 23.0 °C | 6E-7 - 7.5E-7 Ω·m Show Material materials with Electrical resistivity of 6E-7 - 7.5E-7 Ω·m | Typical for Ferritic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.2 - 0.27 % Show Material materials with Carbon of 0.2 - 0.27 % |
Chromium | 16 - 18 % Show Material materials with Chromium of 16 - 18 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Nickel | 1 - 2 % Show Material materials with Nickel of 1 - 2 % |
Phosphorus | 0.05 % Show Material materials with Phosphorus of 0.05 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % |