General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.7 g/cm³ Show Material materials with Density of 7.7 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 200 GPa Show Material materials with Elastic modulus of 200 GPa | Typical for Duplex Stainless Steel |
Elongation | 20.0 °C | 22 % Show Material materials with Elongation of 22 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Duplex Stainless Steel |
Shear modulus | 23.0 °C | 77 GPa Show Material materials with Shear modulus of 77 GPa | Typical for Duplex Stainless Steel |
Tensile strength | 20.0 °C | 650 - 850 MPa Show Material materials with Tensile strength of 650 - 850 MPa | |
Yield strength Rp0.2 | 20.0 °C | 480 MPa Show Material materials with Yield strength Rp0.2 of 480 MPa | |
100.0 °C | 390 MPa Show Material materials with Yield strength Rp0.2 of 390 MPa | ||
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K | |
300.0 °C | 1.4E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.4E-5 1/K | ||
Max service temperature | 300 °C Show Material materials with Max service temperature of 300 °C | Typical for Duplex Stainless Steel | |
Melting point | 1375 - 1450 °C Show Material materials with Melting point of 1375 - 1450 °C | Typical for Duplex Stainless Steel | |
Specific heat capacity | 20.0 °C | 450 J/(kg·K) Show Material materials with Specific heat capacity of 450 J/(kg·K) | |
Thermal conductivity | 50.0 °C | 17 W/(m·K) Show Material materials with Thermal conductivity of 17 W/(m·K) | |
100.0 °C | 18 W/(m·K) Show Material materials with Thermal conductivity of 18 W/(m·K) | ||
Chemical properties
Property | Value |
---|---|
Carbon | 0.03 % Show Material materials with Carbon of 0.03 % |
Chromium | 25 - 27 % Show Material materials with Chromium of 25 - 27 % |
Copper | 1.3 % Show Material materials with Copper of 1.3 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Molybdenum | 3 - 5 % Show Material materials with Molybdenum of 3 - 5 % |
Nickel | 6 - 8 % Show Material materials with Nickel of 6 - 8 % |
Nitrogen | 0.12 - 0.22 % Show Material materials with Nitrogen of 0.12 - 0.22 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |