Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 14.3 g/cm³ Show Supplier Material materials with Dichte of 14.3 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 25 % Show Supplier Material materials with Dehnung of 25 % | min. |
Elastizitätsmodul | 23.0 °C | 124 GPa Show Supplier Material materials with Elastizitätsmodul of 124 GPa | |
Härte, Vickers | 23.0 °C | 120 - 220 [-] Show Supplier Material materials with Härte, Vickers of 120 - 220 [-] | |
Schubmodule | 23.0 °C | 44 GPa Show Supplier Material materials with Schubmodule of 44 GPa | |
Zugfestigkeit | 23.0 °C | 500 - 750 MPa Show Supplier Material materials with Zugfestigkeit of 500 - 750 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.41E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.41E-5 1/K | RT-100 °C |
Schmelzpunkt | 1190 - 1230 °C Show Supplier Material materials with Schmelzpunkt of 1190 - 1230 °C | ||
Wärmeleitfähigkeit | 23.0 °C | 31 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 31 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 5.5 - 6 % IACS Show Supplier Material materials with Specific Electrical conductivity of 5.5 - 6 % IACS | |
Temperaturwiderstandskoeffizient | 23.0 °C | 1.8E-4 1/K Show Supplier Material materials with Temperaturwiderstandskoeffizient of 1.8E-4 1/K |
spezifischer Widerstand | 23.0 °C | 2.87E-7 - 3.13E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 2.87E-7 - 3.13E-7 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding contacts, Slip ring brushes | |
Corrosion properties | Corrosion resistant | |
Other | Oxidation resistant, Ductile, Age hardenable, Wear Resistant, stable contact resistant |