Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 5-230 mm - Sheet: 17x15-254x63.5 mm |
Mechanisch
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 15.0 - 17.5 % Show Supplier Material materials with Chrom of 15.0 - 17.5 % | |
Kohlenstoff | 0.07 % Show Supplier Material materials with Kohlenstoff of 0.07 % | max. |
Kupfer | 3.0 - 5.0 % Show Supplier Material materials with Kupfer of 3.0 - 5.0 % | |
Mangan | 1.0 % Show Supplier Material materials with Mangan of 1.0 % | max. |
Nickel | 3.0 - 5.0 % Show Supplier Material materials with Nickel of 3.0 - 5.0 % | |
Niobium | 0.15 - 0.45 % Show Supplier Material materials with Niobium of 0.15 - 0.45 % | |
Phosphor | 0.025 % Show Supplier Material materials with Phosphor of 0.025 % | max. |
Schwefel | 0.025 % Show Supplier Material materials with Schwefel of 0.025 % | max. |
Silizium | 1.0 % Show Supplier Material materials with Silizium of 1.0 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace | |
Processing history | Solution Annealed |