Wrought Copper Nickel Grade
DEF STAN 02-835 Copper AlloyLeaded Brass
EN 12163 Grade CuZn35Ni3Mn2AlPb R490Acero inoxidable ferrítico
EN 10095 Grade X10CrAlSi25 soft annealed (+A)Acero inoxidable ferrítico
SEW 470 Grade X10CrAlSi25 soft annealed (+A)Nickel Chromium Alloy
DIN 17742 Grade NiCr20TiAl precipitation hardened (+P)Nickel Chromium Iron Alloy
Sanicro® 61Suministrada por:
Alleima (formerly Sandvik Materials Technology)Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R590Acero inoxidable endurecido por precipitación
EN 10270-3 Grade X7CrNiAl17-7 precipitation hardened (+P)Acero inoxidable endurecido por precipitación
EN 10270-3 Grade X7CrNiAl17-7 cold drawnAcero inoxidable endurecido por precipitación
DIN 17224 Grade X 7 CrNiAl 17 7 solution annealed (+AT)Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R540Leaded Brass
EN 12164 Grade CuZn40Mn1Pb1AlFeSn R460Leaded Brass
EN 12164 Grade CuZn40Mn1Pb1AlFeSn R500Leaded Brass
EN 12164 Grade CuZn40Mn1Pb1AlFeSn R520Leaded Brass
EN 12168 Grade CuZn40Mn1Pb1AlFeSn H100Leaded Brass
EN 12167 Grade CuZn39Mn1AlPbSi H110