Coeficiente de dilatación térmica: 1.66E-5 - 1.71E-5 1/K

Quick Comparison

Polyamide 66 (PA66)

Zytel® 70G35HSL NC010

Mezcla de polímeros

VALOX™ FR Resins 865

Polyamide 66 (PA66)

Zytel® 70G35HSLX BK357

Acero inoxidable austenítico

Sandvik 253 MA

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Wrought Copper Nickel Silver Grade

UNS C77000 boway

Suministrada por:

Ningbo Boway Alloy Material

Wrought Copper Nickel Silver Grade

UNS C75200 boway

Suministrada por:

Ningbo Boway Alloy Material

Wrought Copper Nickel Grade

UNS C70260 boway

Suministrada por:

Ningbo Boway Alloy Material

Bronce fosforado

UNS C51900 boway

Suministrada por:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

UNS C19010 boway

Suministrada por:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

UNS C19005 boway

Suministrada por:

Ningbo Boway Alloy Material

Polyamide 66 (PA66)

Zytel® 70G35EF NC010

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TH04

Nickel Chromium Iron Alloy

Sanicro® 28

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Wrought Copper High Copper Alloy

UNS C19210 boway

Suministrada por:

Ningbo Boway Alloy Material

Polyamide 66 (PA66)

Zytel® 70G35EF BK538

Tereftalato de polibutileno (PBT)

LNP™ THERMOTUF™ Compound WF008N

Suministrada por:

Sabic

Compuesto de matriz de polímero termoendurecible

Phenolic NP660 - Sheet

Suministrada por:

Norplex-Micarta

Acero inoxidable austenítico

Alloy 24 / 1.4565 Solution annealed and quenched

Suministrada por:

Hempel Special Metals

Polyamide 66 (PA66)

Zytel® 70G35HSRX BK099
Página 1 de 399