Densidad: 1.4 - 1.53 g/cm³

Quick Comparison

Tereftalato de polibutileno (PBT)

LNP™ THERMOCOMP™ Compound WF006XXP

Suministrada por:

Sabic

Polyamide 46 (PA46)

Stanyl® TW200F6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW241F6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE200F6-FC

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE200F6

Suministrada por:

DSM Engineering Materials

Polyvinylidenefluoride (PVDF)

Kynar Flex® 3120-10

Suministrada por:

Arkema: High Performance Polymers

Polyamide 66 (PA66)

Zytel® 70G43L NC010

Polyamide 4T (PA4T)

ForTii® F11

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

Zytel® 70G35HSL NC010

Polyamide 4T (PA4T)

ForTii® T11

Suministrada por:

DSM Engineering Materials

Polyamide 4T (PA4T)

ForTii® TX1

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW200F8

Suministrada por:

DSM Engineering Materials

Mezcla de polímeros

LNP™ THERMOCOMP™ Compound 6F006I

Suministrada por:

Sabic

Polyamide 46 (PA46)

Stanyl® TW200F6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW241F8

Suministrada por:

DSM Engineering Materials

Policarbonato (PC)

LNP™ THERMOCOMP™ Compound D451RC

Suministrada por:

Sabic

Mezcla de polímeros

VALOX™ FR Resin ENH8530 - Europe

Suministrada por:

Sabic

Polyamide 6T (PA6T)

Zytel® HTN51G35HSL NC010

Poliéter éter cetona (PEEK)

TECACOMP PEEK TRM PVX black 1046944

Suministrada por:

Ensinger GmbH

Mezcla de polímeros

VALOX™ FR Resins 855
Página 1 de 49