General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Bulk density | 0.63 g/cm³ Show Supplier Material materials with Bulk density of 0.63 g/cm³ | EN ISO 60 | |
Density | 1.5 g/cm³ Show Supplier Material materials with Density of 1.5 g/cm³ | ||
Water absorption | 0.1 % Show Supplier Material materials with Water absorption of 0.1 % | DIN EN ISO 62 | max. | 23°C | 50 % r.h. up to saturation |
Mechanical
Property | Value | Testing Standard | Comment |
---|---|---|---|
Compressive modulus | 4100 GPa Show Supplier Material materials with Compressive modulus of 4100 GPa | EN ISO 604 | 1 mm/min |
Compressive strength | 180 MPa Show Supplier Material materials with Compressive strength of 180 MPa | EN ISO 604 | 5 mm/min |
Elastic modulus | 12.5 GPa Show Supplier Material materials with Elastic modulus of 12.5 GPa | DIN EN ISO 527-1 | 50 mm/min |
Elongation | 1.8 % Show Supplier Material materials with Elongation of 1.8 % | DIN EN ISO 527-1 | 50 mm/min |
Flexural modulus | 11.2 GPa Show Supplier Material materials with Flexural modulus of 11.2 GPa | DIN EN ISO 178 | 2 mm/min |
Flexural strain | 2 % Show Supplier Material materials with Flexural strain of 2 % | DIN EN ISO 178 | 2 mm/min |
Flexural strength | 195 MPa Show Supplier Material materials with Flexural strength of 195 MPa | DIN EN ISO 178 | 2 mm/min |
Impact strength, Charpy unnotched | 30 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 30 kJ/m² | DIN EN ISO 179-1eU | |
Tensile strength | 155 MPa Show Supplier Material materials with Tensile strength of 155 MPa | DIN EN ISO 527-1 | 50 mm/min |
Thermal
Property | Value | Testing Standard | Pressure | Comment | |||
---|---|---|---|---|---|---|---|
Coefficient of thermal expansion | 1.3e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.3e-05 1/K | DIN EN ISO 11359-1/2 | at 23-55°C | ||||
2.2e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.2e-05 1/K | DIN EN ISO 11359-1/2 | at 200-300°C | |||||
4.5e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4.5e-05 1/K | DIN EN ISO 11359-1/2 | at 23-55°C, Transverse | |||||
0.000147 1/K Show Supplier Material materials with Coefficient of thermal expansion of 0.000147 1/K | DIN EN ISO 11359-1/2 | at 200-300°C, Transverse | |||||
Glass transition temperature | 143 °C Show Supplier Material materials with Glass transition temperature of 143 °C | DIN 53765 | |||||
Heat deflection temperature | 325 °C Show Supplier Material materials with Heat deflection temperature of 325 °C | ISO-R 75 Method A | 1.8 MPa | ||||
340 °C Show Supplier Material materials with Heat deflection temperature of 340 °C | ISO-R 75 Method B | 0.45 MPa | |||||
Max service temperature | 260 °C Show Supplier Material materials with Max service temperature of 260 °C | Long | |||||
300 °C Show Supplier Material materials with Max service temperature of 300 °C | Short | ||||||
Melting point | 343 °C Show Supplier Material materials with Melting point of 343 °C | DIN 53765 | |||||
Thermal conductivity | 0.5 W/(m·K) Show Supplier Material materials with Thermal conductivity of 0.5 W/(m·K) | DIN EN 821 | through-plane | ||||
0.9 W/(m·K) Show Supplier Material materials with Thermal conductivity of 0.9 W/(m·K) | DIN EN 821 | in-plane | |||||
Flammability | UL94 class V0, DIN IEC 60695-11-10 |
Electrical
Property | Value | Testing Standard |
---|---|---|
Surface resistivity | 14000 Ω/sq Show Supplier Material materials with Surface resistivity of 14000 Ω/sq | DIN EN 61340-2-3 |
Volume resistivity | 1.2e+06 Ω·cm Show Supplier Material materials with Volume resistivity of 1.2e+06 Ω·cm | DIN EN 61340-2-3 |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt mass-flow rate | 20 g/10min Show Supplier Material materials with Melt mass-flow rate of 20 g/10min | DIN EN ISO 1133 | 380°C/5kg |
Melt volume-flow rate | 16 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 16 cm³/10min | DIN EN ISO 1133 | 380°C/5kg |
Shrinkage | 0.27 % Show Supplier Material materials with Shrinkage of 0.27 % | DIN EN ISO 294-4 | |
0.85 % Show Supplier Material materials with Shrinkage of 0.85 % | DIN EN ISO 294-4 | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive industry: Seat (bumper, roll), Steering, Gear (shift handle and bearings), electronics (radar) and Mechanical engineering | |
Color | Black | |
Fillers | Carbon Fiber, PTFE, Graphite | |
Processing methods | Permissible residual moisture content (%): 0.02, drying temperature (°C): 180, drying time (h): 6, mould temperature (°C): 200, material temperature (°C): 400, cylinder/processing temperature (°C): 400 |