Acero bajo en carbono
EN 10025-2 Grade S235JR as-rolled condition (+AR)Suministrada por:
1 proveedor Matmatch
Acero bajo en carbono
EN 10025-2 Grade S235J0 normalized or normalized formed (+N)Suministrada por:
1 proveedor Matmatch
Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Wrought Copper High Copper Alloy
ASTM B251 Grade C17000 TD04Wrought Copper High Copper Alloy
ASTM B196 Grade C17000 TF00