Polyamide 66 (PA66)
RADISTRONG A RV600W 333 BKSuministrada por:
RadiciGroup High Performance PolymersPolyamide 610 (PA610)
RADILON D RV600RKC 306 BKSuministrada por:
RadiciGroup High Performance PolymersPolyamide 66 (PA66)
RADISTRONG AROMA RV600RKC2 306 BKSuministrada por:
RadiciGroup High Performance PolymersGrey Cast Iron
EN 1561 Grade GJL-150 cast conditionCompuesto de matriz cerámica a base de carburos
SIGRASIC® Carbon Fiber Reinforced Silicon Carbide FeltSuministrada por:
SGL Carbon