Special PA 60% glass fibre reinforced, injection moulding grade. Heat stabilized. Black colour.

Product with enhanced mechanical properties, suitable for demanding applications as in case of metal replacement

This material data has been provided by Radici Group.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting StandardThickness

Density

1.73 g/cm³

Show Supplier Material materials with Density of 1.73 g/cm³

dry

ISO 1183

Moisture absorption

0.8 %

Show Supplier Material materials with Moisture absorption of 0.8 %

50% RH

ISO 62

2 mm

Water absorption

3.2 %

Show Supplier Material materials with Water absorption of 3.2 %

ISO 62

2 mm

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

17 GPa

Show Supplier Material materials with Elastic modulus of 17 GPa

50%RH

ISO 527-2/1A

1mm/min

22 GPa

Show Supplier Material materials with Elastic modulus of 22 GPa

dry

ISO 527-2/1A

1mm/min

Elongation

2 %

Show Supplier Material materials with Elongation of 2 %

dry

ISO 527-2/1A

5mm/min

2 %

Show Supplier Material materials with Elongation of 2 %

50%RH

ISO 527-2/1A

5mm/min

Flexural modulus

17 GPa

Show Supplier Material materials with Flexural modulus of 17 GPa

50%RH

ISO 178

2mm/min

21 GPa

Show Supplier Material materials with Flexural modulus of 21 GPa

dry

ISO 178

2mm/min

Flexural strength

320 MPa

Show Supplier Material materials with Flexural strength of 320 MPa

50%RH

ISO 178

2mm/min

390 MPa

Show Supplier Material materials with Flexural strength of 390 MPa

dry

ISO 178

2mm/min

Impact strength, Charpy notched

-30 °C

15 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 15 kJ/m²

dry

ISO 179/1eA

-30 °C

16 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 16 kJ/m²

50%RH

ISO 179/1eA

23 °C

17 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 17 kJ/m²

dry

ISO 179/1eA

23 °C

18 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 18 kJ/m²

50%RH

ISO 179/1eA

Impact strength, Charpy unnotched

-30 °C

83 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 83 kJ/m²

dry

ISO 179/1eU

-30 °C

85 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 85 kJ/m²

dry, 50%RH

ISO 179/1eU

23 °C

85 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 85 kJ/m²

dry, 50%RH

ISO 179/1eU

23 °C

90 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 90 kJ/m²

50%RH

ISO 179/1eU

Tensile strength

190 MPa

Show Supplier Material materials with Tensile strength of 190 MPa

50%RH

ISO 527-2/1A

5mm/min

275 MPa

Show Supplier Material materials with Tensile strength of 275 MPa

dry

ISO 527-2/1A

5mm/min

Thermal

PropertyValueTesting StandardPressureComment

Coefficient of thermal expansion

1.3e-05 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.3e-05 1/K

ISO 11359-1/-2

23°C-55°C

7.3e-05

Show Supplier Material materials with Coefficient of thermal expansion of 7.3e-05

ISO 11359-1/-2

23°C-55°C, Transverse

Heat deflection temperature

245 °C

Show Supplier Material materials with Heat deflection temperature of 245 °C

ISO 75/2Af

2 MPa

Melting point

255 °C

Show Supplier Material materials with Melting point of 255 °C

ISO 11357-1/-3

10°C/min

Flammability

Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3

Electrical

PropertyValueConditionTesting StandardComment

Surface resistivity

1e+10 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq

50%RH

IEC 60093

500V

1e+12 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq

dry

IEC 60093

500V

Volume resistivity

1e+12 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm

50%RH

IEC 60093

500V

1e+14 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+14 Ω·cm

dry

IEC 60093

500V

Rheological Properties

PropertyValueConditionTesting StandardComment

Shrinkage

0.1 %

Show Supplier Material materials with Shrinkage of 0.1 %

dry

ISO 294-4

0.3 %

Show Supplier Material materials with Shrinkage of 0.3 %

dry

ISO 294-4

Transverse

Technological properties

Property
Certifications

RoHS 2011/65/UE

Color

Black

Fillers

60% Glass Fiber

Processing methods

Injection Molding