Aleación de hierro
Kovar® SheetAleación de hierro
Kovar® PlateAleación de hierro
Kovar® Strip/CoilAleación de hierro
Kovar® BarAcero inoxidable austenítico
EN 10088-1 Grade X1CrNiMoCuN25-25-5 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X1CrNiMoCuN25-25-5 solution annealed (+AT)Cast Copper Nickel Grade
DIN 17658 Grade G-CuNi30 MAcero inoxidable endurecido por precipitación
UGI® HT286 Annealed and Cold Drawn and AgedSuministrada por:
UgitechAcero inoxidable endurecido por precipitación
UGI® HT286 Annealed and Cold DrawnSuministrada por:
UgitechAcero inoxidable austenítico
ASTM A453 Grade 651 Class AAcero inoxidable austenítico
EN 10213-4 Grade GX2NiCrMo28-20-2 solution heat-treated and quenchedGrey Cast Iron
EN 13835 Grade GGL-NiCr 30 3 cast conditionAcero inoxidable austenítico
ASTM A182 Grade F347 Solution-AnnealedAcero inoxidable austenítico
ASTM A240 Grade 904L Heat-TreatedDuctile (Nodular) Cast Iron
EN 13835 Grade GGG-NiCr 30 1 cast condition