Calor específico: 472 J/(kg·K)

Quick Comparison

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Chromium Molybdenum Steel

EN 10028-2 Grade 12CrMoV12-10 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMoSi5-5 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMoV9-10 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

ISO 683-1 Grade C45E quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

EN 10083-3 Grade 30MnB5 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Chromium Molybdenum Steel

ASTM A542 Type E Class 4 Quenched and Tempered

Suministrada por:

1 proveedor Matmatch

Chromium Molybdenum Steel

ASTM A387 Grade 12 Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered

Suministrada por:

1 proveedor Matmatch

Nickel Molybdenum Steel

ASTM A387 Grade 11 Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered

Suministrada por:

1 proveedor Matmatch

Chromium Molybdenum Steel

ASTM A542 Type A Class 2 Quenched and Tempered

Suministrada por:

1 proveedor Matmatch

Chromium Molybdenum Steel

ASTM A542 Type D Class 1 Quenched and Tempered

Suministrada por:

1 proveedor Matmatch

Chromium Molybdenum Steel

ASTM A542 Type A Class 1 Quenched and Tempered

Suministrada por:

1 proveedor Matmatch

Chromium Molybdenum Steel

ASTM A542 Type B Class 1 Quenched and Tempered

Suministrada por:

1 proveedor Matmatch

Nickel Chromium Iron Alloy

VDM® Alloy 601

Suministrada por:

VDM Metals

Nickel Chromium Iron Alloy

VDM® Alloy 330

Suministrada por:

VDM Metals

Nickel Chromium Iron Alloy

VDM® Alloy DS*

Suministrada por:

VDM Metals

Aleación alfa-beta

DIN 17851 Grade 3.7185
Página 1 de 115