Resistencia a la tracción: 1270 - 2260 MPa

Quick Comparison

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00

Unclassified Low Alloy Steel

ISO 683-2 Grade 33MnCrB5-2 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Nickel Chromium Iron Alloy

VDM® Alloy 718

Suministrada por:

VDM Metals

Wrought Copper High Copper Alloy

ASTM B196 Grade C17000 TB00

Wrought Copper High Copper Alloy

ASTM B196 Grade C17000 TH04

Aleación alfa-beta

AMS 4918 Grade R56620

Aleación alfa-beta

AMS 4918 Grade R56620

Aleación alfa-beta

AMS 4918 Grade R56620

Wrought Copper High Copper Alloy

ASTM B643 Grade C17200 TH04

Acero inoxidable austenítico

UGI® 209 Solution Annealed

Suministrada por:

Ugitech

Nickel Chromium Molybdenum Steel

Carbodur 6587 Blank Hardened

Suministrada por:

Deutsche Edelstahlwerke (DEW)

Nickel Chromium Molybdenum Steel

Firmodur 6582 QT

Suministrada por:

Deutsche Edelstahlwerke (DEW)

Chromium Molybdenum Steel

Firmodur 7225 QT

Suministrada por:

Deutsche Edelstahlwerke (DEW)

Chromium Molybdenum Steel

Firmodur 7227 QT

Suministrada por:

Deutsche Edelstahlwerke (DEW)

Acero inoxidable endurecido por precipitación

Acidur 4542 P1070

Suministrada por:

Deutsche Edelstahlwerke (DEW)

Acero inoxidable martensítico

UGI 4418 AIR QT1150

Suministrada por:

Ugitech

Acero inoxidable endurecido por precipitación

UGI® 4545 AIR H900

Suministrada por:

Ugitech

Wrought Copper High Copper Alloy

ASTM B197 Grade C17300 TH04