ISO 4957 Grade X165CrMoV12 soft annealed (+A)

Want to keep this datasheet? Save it now in your required format

Description

Properties: - good dimensional stability - high wear resistance - able for nitriding Application: - for high speedcut and stamping tool for sheet thickness up to 5 mm, roll and blade knifes up to 4 mm sheet thickness - cold draw dies - flanges, bead and truing rolls for the continuous profile and tubing production from strip steel - tools for cold working of screws, nuts and rivets - machining tools for wood

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.68 g/cm³

Show Material materials with Density of 7.68 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

215 GPa

Show Material materials with Elastic modulus of 215 GPa

100.0 °C

211 GPa

Show Material materials with Elastic modulus of 211 GPa

200.0 °C

204 GPa

Show Material materials with Elastic modulus of 204 GPa

300.0 °C

198 GPa

Show Material materials with Elastic modulus of 198 GPa

400.0 °C

191 GPa

Show Material materials with Elastic modulus of 191 GPa

500.0 °C

182 GPa

Show Material materials with Elastic modulus of 182 GPa

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Tool And Machining Steel

Shear modulus

23.0 °C

79 GPa

Show Material materials with Shear modulus of 79 GPa

Typical for Tool And Machining Steel

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

-100.0 °C

8.6E-6 1/K

Show Material materials with Coefficient of thermal expansion of 8.6E-6 1/K

20.0 °C

1.01E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.01E-5 1/K

100.0 °C

1.07E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.07E-5 1/K

200.0 °C

1.13E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.13E-5 1/K

300.0 °C

1.18E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.18E-5 1/K

400.0 °C

1.22E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.22E-5 1/K

500.0 °C

1.25E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.25E-5 1/K

Unlock all property charts

Melting point

1370 - 1425 °C

Show Material materials with Melting point of 1370 - 1425 °C

Typical for Tool And Machining Steel

Specific heat capacity

20.0 °C

439 J/(kg·K)

Show Material materials with Specific heat capacity of 439 J/(kg·K)

Thermal conductivity

20.0 °C

31.9 W/(m·K)

Show Material materials with Thermal conductivity of 31.9 W/(m·K)

100.0 °C

31.5 W/(m·K)

Show Material materials with Thermal conductivity of 31.5 W/(m·K)

200.0 °C

30.9 W/(m·K)

Show Material materials with Thermal conductivity of 30.9 W/(m·K)

300.0 °C

29.7 W/(m·K)

Show Material materials with Thermal conductivity of 29.7 W/(m·K)

400.0 °C

28.6 W/(m·K)

Show Material materials with Thermal conductivity of 28.6 W/(m·K)

500.0 °C

27.6 W/(m·K)

Show Material materials with Thermal conductivity of 27.6 W/(m·K)

Unlock all property charts

Thermal diffusivity

20.0 °C

9.5 mm²/s

Show Material materials with Thermal diffusivity of 9.5 mm²/s

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

4.53E-7 Ω·m

Show Material materials with Electrical resistivity of 4.53E-7 Ω·m

100.0 °C

5.15E-7 Ω·m

Show Material materials with Electrical resistivity of 5.15E-7 Ω·m

200.0 °C

5.96E-7 Ω·m

Show Material materials with Electrical resistivity of 5.96E-7 Ω·m

300.0 °C

6.95E-7 Ω·m

Show Material materials with Electrical resistivity of 6.95E-7 Ω·m

400.0 °C

7.98E-7 Ω·m

Show Material materials with Electrical resistivity of 7.98E-7 Ω·m

500.0 °C

9.08E-7 Ω·m

Show Material materials with Electrical resistivity of 9.08E-7 Ω·m

Unlock all property charts

Chemical properties

PropertyValue

Carbon

1.55 - 1.75 %

Show Material materials with Carbon of 1.55 - 1.75 %

Chromium

11 - 12 %

Show Material materials with Chromium of 11 - 12 %

Manganese

0.2 - 0.4 %

Show Material materials with Manganese of 0.2 - 0.4 %

Molybdenum

0.5 - 0.7 %

Show Material materials with Molybdenum of 0.5 - 0.7 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.25 - 0.4 %

Show Material materials with Silicon of 0.25 - 0.4 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Tungsten

0.4 - 0.6 %

Show Material materials with Tungsten of 0.4 - 0.6 %

Vanadium

0.1 - 0.5 %

Show Material materials with Vanadium of 0.1 - 0.5 %