Acero inoxidable austenítico
DIN 17440 Grade X2CrNiMoN17-13-3 solution heat-treated and quenchedAcero inoxidable austenítico
DIN 17440 Grade X2CrNiMoN17-13-5 solution heat-treated and quenchedAcero inoxidable austenítico
DIN 17440 Grade X2CrNiMoN17-13-3 quenched (+Q)Aleación casi alfa
DIN 17850 Grade Ti3Pd AnnealedAleación casi alfa
VdTÜV WB 230-3 Grade TiNi0.8Mo0.3 AnnealedSuministrada por:
2 proveedores de Matmatch
Acero inoxidable austenítico
EN 10216-5 Grade X3CrNiMoN17-13 solution annealed (+AT)Acero inoxidable austenítico
DIN 1654-5 Grade X2CrNiMoN17-13-3 quenched (+Q)Acero inoxidable dúplex
EN 10095 Grade X10NiCrSiNb35-22 solution annealed (+AT)Acero inoxidable austenítico
DIN 17460 Grade X3CrNiMoN17-13 solution annealed (+AT)Superaustenitic Stainless Steel
EN 10095 Grade X10NiCrSi35-19 solution annealed (+AT)Nickel Chromium Molybdenum Alloy
DIN 17744 Grade NiMo16Cr16Ti solution heat-treated and quenchedAcero inoxidable austenítico
EN 10088-1 Grade X1NiCrMoCuN25-20-7 solution heat-treated and quenchedNickel Chromium Molybdenum Alloy
DIN 17744 Grade NiMo16Cr15W solution heat-treated and quenched