HMWPE ISO-TECH

Alternative and trade names
ISO-LEN® 500
Want to keep this datasheet? Save it now in your required format

Description

ISO-LEN® 500 is manufactured in sintering presses using high-molecular-weight raw materials. It is used in a wide variety of shapes and colours in various industries. In addition to its good sliding characteristics, its good abrasion resistance is helpful in many different applications. The key features are:


  • Good sliding coefficient
  • Good abrasion resistance
  • Odourless and tasteless
  • Related Standards

    This material data has been provided by ISO-TECH Kunststoff GmbH.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValueComment

    Coefficient of friction

    0.25 [-]

    Show Supplier Material materials with Coefficient of friction of 0.25 [-]

    DIN 53375, B, Against dry running steel

    Density

    0.95 g/cm³

    Show Supplier Material materials with Density of 0.95 g/cm³

    ISO 1183

    Water absorption

    0.01 %

    Show Supplier Material materials with Water absorption of 0.01 %

    max., ISO 62

    Mechanical

    PropertyValueComment

    Elastic modulus

    1 GPa

    Show Supplier Material materials with Elastic modulus of 1 GPa

    ISO 527

    Elongation

    700 %

    Show Supplier Material materials with Elongation of 700 %

    min., ISO 527

    Elongation at yield

    9 %

    Show Supplier Material materials with Elongation at yield of 9 %

    ISO 527

    Flexural strength

    22 MPa

    Show Supplier Material materials with Flexural strength of 22 MPa

    ISO 178

    Hardness, Shore D

    64 [-]

    Show Supplier Material materials with Hardness, Shore D of 64 [-]

    DIN 53505

    Impact strength, Charpy notched

    29 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy notched of 29 kJ/m²

    ISO 179

    Tear strength

    31 kN/m

    Show Supplier Material materials with Tear strength of 31 kN/m

    ISO 527

    Yield strength

    22 MPa

    Show Supplier Material materials with Yield strength of 22 MPa

    ISO 527

    Impact strength, Charpy unnotched

    No break, ISO 179

    Thermal

    PropertyValuePressureComment

    Coefficient of thermal expansion

    0.00015 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 0.00015 1/K

    DIN 53752

    Heat deflection temperature

    69 °C

    Show Supplier Material materials with Heat deflection temperature of 69 °C

    0.45 MPa

    Max service temperature

    90 °C

    Show Supplier Material materials with Max service temperature of 90 °C

    Longterm

    Long

    Short

    Min service temperature

    -50 °C

    Show Supplier Material materials with Min service temperature of -50 °C

    Longterm

    Thermal conductivity

    0.42 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 0.42 W/(m·K)

    DIN 52612

    Vicat softening temperature

    80 °C

    Show Supplier Material materials with Vicat softening temperature of 80 °C

    ISO 306, VST B50

    Flammability

    HB UL 94

    Electrical

    PropertyValueComment

    Dielectric constant

    2.35 [-]

    Show Supplier Material materials with Dielectric constant of 2.35 [-]

    DIN 53483

    Dielectric strength

    17 kV/mm

    Show Supplier Material materials with Dielectric strength of 17 kV/mm

    VDE 0303

    Loss tangent

    0.0003 [-]

    Show Supplier Material materials with Loss tangent of 0.0003 [-]

    DIN 53483

    Surface resistivity

    1e+16 Ω/sq

    Show Supplier Material materials with Surface resistivity of 1e+16 Ω/sq

    min., VDE 0303

    Volume resistivity

    1e+15 Ω·cm

    Show Supplier Material materials with Volume resistivity of 1e+15 Ω·cm

    min., VDE 0303

    Technological properties

    Property
    Application areas

    Cutting boards, linings and work benches

    Certifications

    Food Contact: FDA and EU 10/2011, RoHS,REACH

    UV resistance

    Partly