General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 1.41 g/cm³ Show Supplier Material materials with Densidad of 1.41 g/cm³ | ISO 1183 |
Moisture absorption | 20.0 °C | 2.65 % Show Supplier Material materials with Moisture absorption of 2.65 % | ISO 62, after 24h |
Viscosity number | 145 cm³/gr Show Supplier Material materials with Viscosity number of 145 cm³/gr | ISO 307, 1157, 1628 | |
Índice límite de óxigeno | 20.0 °C | 20 % Show Supplier Material materials with Índice límite de óxigeno of 20 % | ISO 4589-1/-2 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 20.0 °C | 4 % Show Supplier Material materials with Elongación of 4 % | ISO 527-1/-2 |
120.0 °C | 7.5 % Show Supplier Material materials with Elongación of 7.5 % | ISO 527-1/-2 | |
160.0 °C | 7.5 % Show Supplier Material materials with Elongación of 7.5 % | ISO 527-1/-2 | |
180.0 °C | 7.5 % Show Supplier Material materials with Elongación of 7.5 % | ISO 527-1/-2 | |
200.0 °C | 7.5 % Show Supplier Material materials with Elongación of 7.5 % | ISO 527-1/-2 | |
Módulo de flexión | 20.0 °C | 9 GPa Show Supplier Material materials with Módulo de flexión of 9 GPa | ISO 178 |
120.0 °C | 4.7 GPa Show Supplier Material materials with Módulo de flexión of 4.7 GPa | ISO 178 | |
160.0 °C | 3.9 GPa Show Supplier Material materials with Módulo de flexión of 3.9 GPa | ISO 178 | |
Módulo elástico | 20.0 °C | 10 GPa Show Supplier Material materials with Módulo elástico of 10 GPa | ISO 527-1/-2 |
120.0 °C | 5.5 GPa Show Supplier Material materials with Módulo elástico of 5.5 GPa | ISO 527-1/-2 | |
160.0 °C | 5 GPa Show Supplier Material materials with Módulo elástico of 5 GPa | ISO 527-1/-2 | |
180.0 °C | 4.4 GPa Show Supplier Material materials with Módulo elástico of 4.4 GPa | ISO 527-1/-2 | |
200.0 °C | 4 GPa Show Supplier Material materials with Módulo elástico of 4 GPa | ISO 527-1/-2 | |
Resistencia a la flexión | 20.0 °C | 300 MPa Show Supplier Material materials with Resistencia a la flexión of 300 MPa | ISO 178 |
120.0 °C | 160 MPa Show Supplier Material materials with Resistencia a la flexión of 160 MPa | ISO 178 | |
160.0 °C | 130 MPa Show Supplier Material materials with Resistencia a la flexión of 130 MPa | ISO 178 | |
Resistencia a la tracción | 20.0 °C | 210 MPa Show Supplier Material materials with Resistencia a la tracción of 210 MPa | ISO 527-1/-2 |
120.0 °C | 110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | ISO 527-1/-2 | |
160.0 °C | 100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | ISO 527-1/-2 | |
180.0 °C | 95 MPa Show Supplier Material materials with Resistencia a la tracción of 95 MPa | ISO 527-1/-2 | |
200.0 °C | 90 MPa Show Supplier Material materials with Resistencia a la tracción of 90 MPa | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | ISO 179/1eU |
23.0 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | ISO 179/1eU | |
Resistencia al choque, ensayo Charpy no entallado | -30.0 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | ISO 179/1eU |
23.0 °C | 80 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 80 kJ/m² | ISO 179/1eU | |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 11 kJ/m² | ISO 180/1A |
23.0 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 12 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | |||
Ball pressure temperature | 285 °C Show Supplier Material materials with Ball pressure temperature of 285 °C | ||||
Coeficiente de dilatación térmica | 20.0 °C | 2.5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.5E-5 1/K | ISO 11359-1/-2 | ||
Coeficiente de dilatación térmica transversal | 20.0 °C | 6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 6E-5 1/K | ISO 11359-1/-2 | ||
Heat deflection temperature, 0.45 MPa | 290 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 290 °C | ISO 75-1/-2 | |||
Heat deflection temperature, 1.80 MPa | 290 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 290 °C | ISO 75-1/-2 | |||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | UL 746B, Thickness 0.9, 3mm | |||
Relative temperature index, mechanical impact | 120140 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 120140 °C | UL 746B, respectively for 0.9 and 3mm thickness | |||
Relative temperature index, mechanical strength | 120140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 120140 °C | UL 746B, respectively for 0.9 and 3mm thickness | |||
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | ISO 11357-1/-3, 10°C/min | |||
Temperatura de reblandecimiento Vicat | 290 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 290 °C | ISO 306, 50°C/h 50N | |||
Glow Wire Flammability Index (GWFI) | 960°C at 3mm and 650°C at 0.75mm, IEC 60695-2-1 | ||||
Glow Wire Ignition Temperature (GWIT) | 725°C at 3mm and. 700°C at 0.75mm, IEC 60695-2-13 | ||||
Inflamabilidad | for thickness 1.5 and 0.75mm: HB, UL recognition: Yes, IEC 60695-11-10 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 20.0 °C | 4 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 4 [-] | IEC 60250 |
Constante dieléctrica, 100 Hz | 20.0 °C | 4.3 [-] Show Supplier Material materials with Constante dieléctrica, 100 Hz of 4.3 [-] | IEC 60250 |
Dissipation factor, 100Hz | 20.0 °C | 7E-3 [-] Show Supplier Material materials with Dissipation factor, 100Hz of 7E-3 [-] | IEC 60250 |
Dissipation factor, 1MHz | 20.0 °C | 0.02 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.02 [-] | IEC 60250 |
Resistividad eléctrica | 20.0 °C | 1.00E+14 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.00E+14 Ω·m | IEC 60093 |
Rigidez dieléctrica | 20.0 °C | 30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | IEC 60243-1 |
Índice de seguimiento comparativo | 20.0 °C | 300 V Show Supplier Material materials with Índice de seguimiento comparativo of 300 V | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Contracción | 20.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | Sim. to ISO 294-4 | ||
Contracción transversal | 20.0 °C | 1.3 % Show Supplier Material materials with Contracción transversal of 1.3 % | Sim. to ISO 294-4 | ||
Density of melt | 1.21 g/cm³ Show Supplier Material materials with Density of melt of 1.21 g/cm³ | ||||
Eff. thermal diffusivity | 0.11 mm²/s Show Supplier Material materials with Eff. thermal diffusivity of 0.11 mm²/s | ||||
Specific heat capacity melt | 2200 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2200 J/(kg·K) | ||||
Thermal conductivity of melt | 0.3 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.3 W/(m·K) | ||||
Spiral flow length | 1.0 mm 800 bar: 100mm, 1.0 mm 900 bar: 110mm, 1.0 mm 1000 bar: 120mm, 0.5mm 1200 bar: 33mm, 0.5 mm 1600 bar: 44mm, 0.5 mm 2000 bar: 76mm |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive Bearing Cages, Automotive Connectors, Automotive e-motor Bobbins, Bobbins, Brushholders (electrical components), Brushholders (electro motors), Charge Air Cooler Caps, Coil insulation, DRL sockets, E-Boxes, E-motor electric insulation, Endlaminates (electro motors), Fuse Holders, Hot Charged Air Ducts, Lawnmower Muffler Components, Lawnmower Trimmer Muffler, MTF/DMF Components, Positition Sensor, Self propelled lawnmower transmission gears, Speed Sensor, Start/Stop: Alternator and Starter parts, Suspension System Top Mounts, Temperature Sensor, Torque Convertor Components | |
Fillers | 30% Glass Fiber |